SA182 F22 Cl.3 " `8 _; j# ]4 M4 h b* G
C Mn P S Si Cr Mo 7 U2 M! {7 A& C$ f
0.05-0.15 0.30-0.60 0.040 0.040 0.50 2.00-2.50 0.87-1.13/ u3 t n. l2 G# i3 I% m
# j- I0 B$ [, T3 @8 ~9 v+ E
Tensile strength :515MPa ; i/ Z# g2 Y1 q! o Yield strength : 310MPa